Thomas A. Edison's Adventures in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thomas A. Edison's Adventures in Concrete

Author(s): Raymond C. Heun and Harry R. Moss

Publication: Concrete International

Volume: 9

Issue: 1

Appears on pages(s): 12-14

Keywords: garages; history; portland cements; reinforced concrete; Construction

DOI:

Date: 1/1/1987

Abstract:
Edison's ideas about low-cost concrete housing are discussed. His construction of a prototype garage is described, along with his role in the development of cement production, reinforced concrete construction, and cement tinting and painting in the United States.