China: Contrasts in concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: China: Contrasts in concrete

Author(s): Jerry Holland

Publication: Concrete International

Volume: 11

Issue: 7

Appears on pages(s): 18-24

Keywords: bridges (structures); buildings; concrete dams; concrete construction; precast concrete; reinforced concrete; reviews; Construction

DOI:

Date: 7/1/1989

Abstract:
Describes the use of concrete materials, design, and construction in the People's Republic of China, from the decidedly primitive to structures and equipment as advanced as any to be found in North America.