Progress in CLSM: Continuing Innovation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Progress in CLSM: Continuing Innovation

Author(s): Bruce W. Ramme

Publication: Concrete International

Volume: 19

Issue: 5

Appears on pages(s): 32-33

Keywords: admixtures; backfilling; low-strength materials; soil-cements; standards

DOI:

Date: 5/1/1997

Abstract:
Starting where the technical report on Controlled Low-Strength Materials (CLSM) prepared by ACI Committee 229 and published in 1994 leaves off, this summary provides updated information on technical developments, material properties, mix proportioning, and major recent construction projects. A discussion of the ASTM standards that monitor the consistency and quality of CLSM is outlined. Predictable engineering properties and labor saving features are making CLSM the best choice for numerous applications.