Simple Approach to Precast Beam-Column Connection Assemblies

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simple Approach to Precast Beam-Column Connection Assemblies

Author(s): G. S. Cheok and H. S. Lew

Publication: Symposium Paper

Volume: 128

Issue:

Appears on pages(s): 1363-1384

Keywords: beam-column frame; connections; cyclic loads; ductility; failure; flexural strength; joints (junctions); post-tensioning; precast concrete; reinforced concrete; structural design; Design

DOI: 10.14359/3295

Date: 11/1/1991

Abstract:
An experimental study of precast concrete beam-column connection assemblies is presented. The study was initiated to provide data for the development of a rational design procedure for such connections in high-seismic regions. The objective of the study is to develop a moment-resistant precast concrete connection that is economical and easily constructed. All test specimens were 1/3-scale models of the prototype. The monolithic concrete specimens were designed to 1985 Uniform Building Code (UBC) seismic zone 2 and 4 criteria. The designs of the precast specimens were similar to those for the monolithic specimens designed to UBC seismic zones 2 and 4. Results from the monolithic specimens provide a benchmark for comparison with results from the precast tests. Comparisons of the performances of the monolithic beam-column connections with those of the precast, post-tensioned connections were based on the connection strength, energy absorbed, ductility, and failure mode for the two types of beam-column connections.