Confinement of Reinforced Concrete Columns With Welded Wire Fabric

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Confinement of Reinforced Concrete Columns With Welded Wire Fabric

Author(s): Salim R. RazviI and Murat Saatcioglu

Publication: Structural Journal

Volume: 86

Issue: 5

Appears on pages(s): 615-623

Keywords: columns (supports); confined concrete; earthquake resistant structures; reinforced concrete; reinforcing steels; structural design; tests; welded wire fabric; Design

DOI: 10.14359/3294

Date: 9/1/1989

Abstract:
The behavior of reinforced concrete columns confined with welded-wire fabric was investigated. Thirty-four small-scale specimens with different reinforcement arrangements, including four corner bars as longitudinal reinforcement and various combinations of welded-wire fabric and tie steel as lateral reinforcement, were tested under concentric loading. The results indicate that welded-wire fabric can be effective in confining the core concrete, resulting in significant improvements in strength and ductility of columns. This improvement, which is achieved with a relatively small percentage of steel, is equivalent to that achieved with closely spaced tie and longitudinal reinforcement with a considerably larger steel percentage. Although some practical problems remain, welded-wire fabric can potentially be used in earthquake-resistant structures as confinement reinforcement.