Evaluation, Repair and Reinforcement of an Ultra-Thin, Two-Way Flat Slab With Drop panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation, Repair and Reinforcement of an Ultra-Thin, Two-Way Flat Slab With Drop panels

Author(s): Steven G. Provenghi and Gregg E. Brandow

Publication: Symposium Paper

Volume: 128

Issue:

Appears on pages(s): 1277-1292

Keywords: concrete panels; cracking (fracturing); flat concrete slabs; inspection; nondestructive testing; parking structures; post-tensioning; plastics, polymers and resins; reinforced concrete; repairs; strengthening; structural design; trusses; Design

DOI: 10.14359/3272

Date: 11/1/1991

Abstract:
This is an actual case-study of a four-story reinforced concrete parking structure with ultra-thin, two-way flat slabs with drop panels. The slabs were 4.50 in. thick on bays as large as 27 x 27 ft with midspan deflections as much as 5.50 in. The evaluation included physical inspections to evaluate crack patterns as well as nondestructive tests to locate reinforcing steel and full-scale load tests per ACI recommendations to evaluate the strength of the structural slab. Recommendations for repair and strengthening were accomplished by a combination of external post-tensioning with king-post type trussing below the floor slabs and with a gravity-fed polymer repair of the structural cracks found within the slab.