Properties of Polyaramid Ropes and Implications for Their Use as External Prestressing Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Polyaramid Ropes and Implications for Their Use as External Prestressing Tendons

Author(s): C. J. Burgoyne

Publication: Symposium Paper

Volume: 120

Issue:

Appears on pages(s): 107-124

Keywords: beams (supports); corrosion resistance; creep properties; durability; fatigue (materials); modulus of elasticity; plastics, polymers and resins; prestressed concrete; prestressing; strength; stress relaxation; thermal properties; Design

DOI: 10.14359/3234

Date: 6/1/1990

Abstract:
Paper describes the properties of parallel-lay ropes with a polyaramid (Kelvar 49) core, with particular reference to the long-term properties that are important to the designers of prestressing systems. The anchorage and prestressing systems are described, and results are given for stress-strain, relaxation, creep, stress-rupture, and fatigue behavior. Durability and thermal response are also considered, and it is inferred that the lack of corrosion, in addition to the high strength and high stiffness, makes these materials ideal for use as prestressing tendons where the concrete cannot be used to provide corrosion protection to steel. Descriptions are given of tests on beams prestressed with external tendons, showing that a ductile response can be achieved in a beam made from two brittle materials. It is concluded that these materials will extend the range of structures that can be built with prestressed concrete, and will at last allow the realization of the full potential of externally prestressed concrete.