Design of High-Strength Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of High-Strength Concrete Columns

Author(s): B. Vijaya Rangan, P. Saunders, and E. J. Seng

Publication: Symposium Paper

Volume: 128

Issue:

Appears on pages(s): 851-862

Keywords: columns (supports); compressive strength; structural design; high-strength concretes; reinforced concrete; slenderness ratio; strength; Design

DOI: 10.14359/3206

Date: 11/1/1991

Abstract:
The results obtained from tests conducted on high-strength concrete columns are reported. The experimental program comprised ten axially loaded short columns and six slender columns subjected to axial compression and bending moment. The main test parameters in the case of short columns are the area and the type of lateral reinforcement, whereas the eccentricity of the axial thrust is the major variable in the slender column tests. The paper also includes methods of calculating the strengths of reinforced concrete columns made of high-strength concrete. The calculated strengths agree closely with the test values.