Designing Spillways to Prevent Cavitation Damage

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Designing Spillways to Prevent Cavitation Damage

Author(s): Kathleen H. Frizell and Brent W. Mefford

Publication: Concrete International

Volume: 13

Issue: 5

Appears on pages(s): 58-64

Keywords: aeration; cavitation; dams; spillways; structural design; surface roughness; tolerances (mechanics); Design

DOI:

Date: 5/1/1991

Abstract:
By following the history of cavitation prevention associated with the spillways at Hoover Dam, a general perspective is obtained for how the U.S. Bureau of Reclamation's philosophy on flow surface tolerances and design have changed. These experiences, combined with research on cavitation and alternative spillway designs, have refocused ideas away from requiring very smooth flow surfaces. Research on step spillway designs has prompted the idea that designing in very large roughnesses in the form of steps may yield benefits not only for energy dissipation but also for cavitation prevention.