Title: Market Tower--Indianapolis, Indiana

Author(s): Bill L. Gunin

Publication: Concrete International

Volume: 11

Issue: 1

Appears on pages(s): 31-34

Keywords: costs; framing systems; high-rise buildings; lateral pressure; office buildings; reinforced concrete; structural design; Design

DOI:

Date: 1/1/1989

Abstract:
Market Tower in Indianapolis, Indiana, is a 32-story, 568,000-ftý (52,800-mý) office tower. The design of this building successfully integrates the creative synthesis of architectural design with cost-effective structural concepts. Conventionally reinforced concrete construction using wide-module pan joists for the floor framing along with shearwall/partial tube interaction for lateral load resistance best met the owner's functional and budgetary requirements.




  