Fast Track Concrete for Pavement Repairs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fast Track Concrete for Pavement Repairs

Author(s): Farhad Ansari, Allyn Luke, Nicholas P. Vitillo, Norman Blank and Ibrahim Turhan

Publication: Concrete International

Volume: 19

Issue: 5

Appears on pages(s): 24-29

Keywords: accelerating agents; compressive strength; high-strength concretes; mix paving; proportioning; tests

DOI:

Date: 5/1/1997

Abstract:
The development and testing of two high early-strength concrete mixes is discussed. For minimal traffic disruption, the fast track concrete developed was used in full-depth repair of jointed concrete slabs on an interstate highway in New Jersey. Type I portland cement and a nonchloride-based hardening accelerator were employed in the production of the fast track concrete. A comprehensive experimental program was implemented for examining the strength gain capability as well as the practicality of these mixes for field implementation.