Behavior and Strength of Concrete Masonry Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior and Strength of Concrete Masonry Walls

Author(s): Salah E. E. El-Metwally, Ashraf F. Ashour and W. F. Chen

Publication: Structural Journal

Volume: 88

Issue: 1

Appears on pages(s): 42-48

Keywords: axial loads; bearing capacity; compressive strength; deflection; eccentricity; masonry load-bearing walls; masonry walls; moment-curvature relationship; slenderness ratio; stability; stress-strain relationships; structural analysis; Design.

DOI: 10.14359/3095

Date: 1/1/1991

Abstract:
Describes an analysis method for predicting the bearing capacity of concrete masonry walls using the Newmark integration technique but extended here to account for the softening behavior of the wall. In this study, the


ALSO AVAILABLE IN:

Electronic Structural Journal