Modeling Earthquake Response of Concrete Masonry Building Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling Earthquake Response of Concrete Masonry Building Structures

Author(s): Daniel P. Abrams and Thomas J. Paulson

Publication: Structural Journal

Volume: 88

Issue: 4

Appears on pages(s): 475-485

Keywords: buildings; cracking (fracturing); damping; dynamic tests; earthquake-resistant structures; laboratories; lateral pressure; masonry; models; tests; Design

DOI: 10.14359/3093

Date: 7/1/1991

Abstract:
Discusses considerations involved with modeling concrete masonry building structures at one-quarter scale and reports on tests carried out to evaluate mechanical properties of reduced-scale masonry materials. Procedures used to design and test two different three-story building structures to failure on a shaking table are also presented. Samples of dynamic response are presented to demonstrate the relevance of using scale models for earthquake engineering research.