Optimized Direct Design of Reinforced Concrete Columns With Uniaxial Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Optimized Direct Design of Reinforced Concrete Columns With Uniaxial Loads

Author(s): J. Y. Richard Yen

Publication: Structural Journal

Volume: 87

Issue: 3

Appears on pages(s): 247-251

Keywords: axial loads; bending; columns (supports); computer programs; microcomputers; optimization; reinforced concrete; structural design; Design

DOI: 10.14359/3089

Date: 5/1/1990

Abstract:
The aim of this research is to provide an efficient and direct solution scheme for use in computer-aided design on uniaxially loaded reinforced concrete short columns. Complete section strength equations were derived with two variables, namely, steel ratio {rho} and position of neutral axis c. Solutions were obtained quickly with multivariable iteration techniques and the minimum longitudinal steel. This method is reliable and can be used with any size of computer. In fact, a microcomputer can be used to handle the design of thousands of reinforced columns in only a few seconds.