Fracture Mechanics Approaches to Modeling the Pullout of Anchor Bolts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fracture Mechanics Approaches to Modeling the Pullout of Anchor Bolts

Author(s): L. Elfgren and S. E. Swartz

Publication: Symposium Paper

Volume: 134

Issue:

Appears on pages(s): 63-78

Keywords: anchors (fasteners); cracking (fracturing); crack propagation; damage; finite element method; fracture properties; models; research; Design

DOI: 10.14359/3081

Date: 9/1/1992

Abstract:
Summarizes and presents preliminary results of a round-robin analysis of anchor bolts organized by RILEM TC 90-FMA, Fracture Mechanics of Concrete-Applications. The analyses employed finite element models using fracture mechanics approaches for the most part. The assumptions used in establishing the material/cracking models varied with investigator and included linear elastic fracture mechanics (LEFM), the fictitious crack model (FCM) with linear softening or non-linear softening, a fixed crack line, a variable crack line with non-rotating cracks or rotating cracks. Crack propagation was determined using Mode I parameters, in some cases, with consideration of mixed mode behavior.




  