Suggested Analysis and Design Procedures for Combined Footings and Mats

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Suggested Analysis and Design Procedures for Combined Footings and Mats

Author(s): ACI Committee 336

Publication: Structural Journal

Volume: 85

Issue: 3

Appears on pages(s): 304-324

Keywords: concretes; earth pressure; footings; foundations; loads (forces); mat foundations; reinforced concrete; soil mechanics; stresses; structural analysis; structural design; Design

DOI: 10.14359/3044

Date: 5/1/1988

Abstract:
Report deals with the design of foundations carrying more than a single column or wall load. These foundations are called combined footings and mats. Although primarily concerned with the structural aspects of the design, considerations of soil mechanics cannot be eliminated and the designer should focus on the important interrelation of the two fields in connection with the design of such structural elements. This report is limited to vertical effects of all loading conditions and excludes slabs-on-grade.


ALSO AVAILABLE IN:

Electronic Structural Journal