Title: Spreadsheet Application for Prestressed Concrete Bridge Girder Design

Author(s): Fernando E. Fagundo and David W. Garmizo

Publication: Concrete International

Volume: 12

Issue: 12

Appears on pages(s): 34-38

Keywords: beams (supports); bridges (structures); computer programs; deflection; flexural strength; microcomputers; prestressed concrete; prestressing steels; shear strength; stresses; structural design; Design

DOI:

Date: 12/1/1990

Abstract:
Describes a spreadsheet developed for preliminary design of prestressed concrete bridge girders.