Redistribution of Concrete Stresses Due to Creep after Change of Structural System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Redistribution of Concrete Stresses Due to Creep after Change of Structural System

Author(s): Troels Brondum-Nielsen

Publication: Structural Journal

Volume: 87

Issue: 4

Appears on pages(s): 393-396

Keywords: bending moments; circular prestressing; creep properties; prestressed concrete; stress analysis; stress relaxation; structural design; tanks (containers); Design

DOI: 10.14359/3036

Date: 7/1/1990

Abstract:
Artificially imposed changes in the structural system may create drastic stress redistributions due to creep (or relaxation of concrete stresses). This important fact has frequently been ignored. This paper illustrates the problem for a typical case: prestressed concrete tanks. This time-dependent stress-strain relationship is assumed to correspond to the 1988 proposal for revision of the CEB-FIP Model Code.