Soil-Structure Interaction--A Brief Overview

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Soil-Structure Interaction--A Brief Overview

Author(s): Arnaldo T. Derecho and Arthur A. Huckelbridge

Publication: Symposium Paper

Volume: 127

Issue:

Appears on pages(s): 239-260

Keywords: dynamic characteristics; dynamic structural analysis; earthquake-resistant structures; foundations; inertia; kinematics; kinetics; soil mechanics; soils; Structural Research

DOI: 10.14359/3016

Date: 10/1/1991

Abstract:
A brief discussion of soil-structure interaction, particularly in terms of its effects on structures subjected to earthquakes, is presented. Factors influencing the degree to which soil-structure interaction modifies the response of structures, when compared to the response of rigid-based structures, are listed. The distinction between inertial and kinematic components of soil-structure interaction is made and the generally beneficial effects of interaction on earthquake structural response is noted. Soil-structures interaction effects are most pronounced in rigid, massive structures founded on compliant soils. Brief mention is made of the uncertainties surrounding the determination of interaction effects on structural response, especially those associated with the effects of nonlinear soil behavior.




  