Observations on the Behavior of Reinforced Concrete Buildings During Earthquakes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Observations on the Behavior of Reinforced Concrete Buildings During Earthquakes

Author(s): Jack P. Moehle and Stephen A. Mahin

Publication: Symposium Paper

Volume: 127

Issue:

Appears on pages(s): 67-90

Keywords: beams (supports); buildings; columns (supports); connections; detailing; earthquake-resistant structures; earthquakes; joints (junctions); frames; flat concrete plates; reinforced concrete; structural design; walls; Structural Research

DOI: 10.14359/3007

Date: 10/1/1991

Abstract:
Observations on the performance of reinforced concrete structures during past earthquakes are summarized and discussed. The review covers observations related to the structural concept, proportioning, and detailing. The review draws from experiences gained during numerous earthquakes, and includes observations of acceptable building performances as well as unacceptable ones. The repeated occurrence of many classes of damage and failure suggests lessons that should be learned.