International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of a Concrete Chimney

Author(s): H. Daryl Richardson and Lloyd E. Rodway

Publication: Concrete International

Volume: 19

Issue: 4

Appears on pages(s): 53-56

Keywords: chimneys; reinforced concrete; strength; structural analysis; tests; x-ray diffraction;

DOI:

Date: 4/1/1997

Abstract:
A detailed engineering assessment of a 32-year-old 300 ft tall, brick-lined reinforced concrete chimney is presented. Tools used for the assessment include infrared photography, Schmidt hammer mapping, x-ray diffraction analysis, strength testing of concrete cylinders, and structural analysis by finite element and classical methods. Design and performance deficiencies are reported, as is the use of high alumina cement concrete not indicated on the engineering drawings. The chimney was found to be suitable for continued service after minor repairs.




  

Edit Module Settings to define Page Content Reviewer