Punching Shear Failure of a Reinforced Concrete Pier Deck Model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Punching Shear Failure of a Reinforced Concrete Pier Deck Model

Author(s): L. J. Malvar

Publication: Structural Journal

Volume: 89

Issue: 5

Appears on pages(s): 569-576

Keywords: bridge decks; failure; piers; reinforced concrete; strains; shear properties; Structural Research

DOI: 10.14359/2990

Date: 9/1/1992

Abstract:
A one-third scale reinforced concrete pier deck model is tested to punching shear failure under a patch load representative of a crane outrigger loading. A three-dimensional nonlinear finite element analysis is carried out to simulate the progressive crack propagation, stiffness degradation, and mode of failure. It is shown that the numerical model is dependent on the concrete constitutive laws used in the post-cracking range.


ALSO AVAILABLE IN:

Electronic Structural Journal