Shear Reinforcement For Deflection Ductility of Flat Plates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Reinforcement For Deflection Ductility of Flat Plates

Author(s): Carl Erik Broms

Publication: Structural Journal

Volume: 87

Issue: 6

Appears on pages(s): 696-705

Keywords: bent-up bars; building codes; deflection; ductility; tests; flat concrete plates; flexural strength; punching shear; reinforcing steels; shear strength; stirrups; structural design; Structural Research

DOI: 10.14359/2988

Date: 11/1/1990

Abstract:
The deflection ductility of flat plates with different types of shear reinforcement is tested. Excellent performance is achieved with a combination of bent bars and stirrups, even at reinforcement ratios exceeding 0.75{rho}b. Code requirements for flat plates are critically reviewed, and design recommendations are given for the bent bar/stirrup reinforcement arrangement.


ALSO AVAILABLE IN:

Electronic Structural Journal