Bamboo-Reinforced Concrete Beams Subjected to Third-Point Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bamboo-Reinforced Concrete Beams Subjected to Third-Point Loading

Author(s): J. K. Kankam, M. Ben-George, and S. H. Perry

Publication: Structural Journal

Volume: 85

Issue: 1

Appears on pages(s): 61-67

Keywords: bamboo; beams (supports); bond (concrete to reinforcement); fibers; reinforced concrete; reinforcing materials; Structural Research

DOI: 10.14359/2981

Date: 1/1/1988

Abstract:
Ten bamboo-reinforced concrete simply supported beams were tested to failure under third-point loading, and six other beams were subjected to long-term loading. Collapse of the 10 beams occurred mostly through diagonal tension failure of the concrete in the shear span; the experimental failure loads averaged 2.4 times the theoretical shear strength of the concrete section alone but only 0.9 times the theoretical shear strength when the effects of both the concrete section and the tension reinforcement were considered. A method based on the analysis of the results is proposed for the design of such beams.


ALSO AVAILABLE IN:

Electronic Structural Journal