Load Balancing: A Comprehensive Solution to Post-Tensioning

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load Balancing: A Comprehensive Solution to Post-Tensioning

Author(s): Bijan O. Aalami

Publication: Structural Journal

Volume: 87

Issue: 6

Appears on pages(s): 662-670

Keywords: flexural strength; limit state design; load balancing method; moments; plasticity; post-tensioning; prestressed concrete; prestressing; serviceability; structural analysis; structural design; Structural Research

DOI: 10.14359/2970

Date: 11/1/1990

Abstract:
Reviews the application of load balancing in a broader context as the emerging standard for analyzing post-tensioned buildings. Terminology, concepts, and current procedures used in the extended scope of load balancing are presented, and the governing relationships are introduced and discussed. The redistribution of elastically computed moments due to limited joint plastification is examined, and numerical examples illustrate the application of load balancing to more complex structures and the importance of faithful representation of balanced loading.


ALSO AVAILABLE IN:

Electronic Structural Journal