Title: T-shaped reinforced concrete members under biaxial bending and axial compression

Author(s): Cheng-Tzu Thomas Hsu

Publication: Structural Journal

Volume: 86

Issue: 4

Appears on pages(s): 460-468

Keywords: axial loads; bending; biaxial loads; columns (supports); compression; computer programs; reinforced concrete; structural analysis; structural design; tests; Structural Research

DOI: 10.14359/2967

Date: 7/1/1989

Abstract:
Presents an experimental and analytical study of T-shaped reinforced concrete members under biaxial bending and axial compression. The strength and deformational behavior of T-shaped reinforced concrete members under biaxial loads monotonically up to failure are explored. The theoretical predictions agree well with the experimental data of 12 test specimens reported herein. Of the total 12 test specimens, 9 were made with normal weight concrete, 1 with fly ash concrete, and 2 with high-strength concrete. The strength interaction curves and load contours of T-shaped members are derived to provide advice for design information.