Microstructural and Mechanical Effects of Latex, Methylcellulose, and Silica Fume on Carbon Fiber Reinforced Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Microstructural and Mechanical Effects of Latex, Methylcellulose, and Silica Fume on Carbon Fiber Reinforced Cement

Author(s): Pu-Woei Chen, Xuli Fu, and D. D. L. Chung

Publication: Materials Journal

Volume: 94

Issue: 2

Appears on pages(s): 147-155

Keywords: carbon; cements; concrete; flexural strength; latex (plastic); silica fume; voids;

DOI: 10.14359/296

Date: 3/1/1997

Abstract:
The effect of methylcellulose, silica fume, and latex on the degree of dispersion of short carbon fibers in cement paste (with water-reducing agent in an amount varying from 0 to 3 percent by weight of cement) was assessed. This degree, as indicated by the ratio of the measured volume of electrical conductivity to the calculated value, and the effectiveness of the fibers in enhancing the tensile/flexural properties attained by using methylcellulose and silica fume were higher than those attained by using methylcellulose alone or latex. Methylcellulose was superior to latex in giving a high degree of fiber dispersion at fiber volume fractions 1 percent, as measured by this technique, but latex resulted in superior tensile-flexural properties and lower content and size of air voids than methylcellulose. With the fiber content fixed at 0.53 vol. percent, the degree of fiber dispersion, as measured by this technique, decreased with increasing latex-cement ratio from 0.05 to 0.30, while the void content attained a minimum at an intermediate latex-cement ratio of 0.15. As a result of the former, the flexural toughness decreased monotonically with increasing latex-cement ratio. As a result of the latter, the flexural strength attained a maximum at an intermediate latex-cement ratio of 0.15. In contrast, both flexural toughness and strength increased monotonically with increasing latex-cement ratio when fibers were absent.