Punching Shear Tests of Half-Scale Reinforced Concrete Flat Plate Models With Spandrel Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Punching Shear Tests of Half-Scale Reinforced Concrete Flat Plate Models With Spandrel Beams

Author(s): M. FalmakiI and Y .C. Loo

Publication: Structural Journal

Volume: 89

Issue: 3

Appears on pages(s): 263-271

Keywords: columns (supports); connections; failure; flat concrete plates; models; punching shear; reinforced concrete; shear strength; torsion; spandrel beams; strength analysis; Structural Research

DOI: 10.14359/2953

Date: 5/1/1992

Abstract:
As part of a long-term research project on the punching shear strength of reinforced concrete flat plates, a series of nine half-scale models representing two adjacent edge and corner panels of a building floor have been tested to failure. The design, fabrication, instrumentation, and ultimate behavior of the models are described and test results are presented. The study indicates that the mechanism of failure of a slab-column-spandrel connection is greatly influenced by the strengths of the slab and beam elements adjoining the front and side column faces, respectively. Based on the information gathered from the failure of the 24 edge and corner column connections, the effects of the strength of the spandrel beam, or torsion strip, and the slab-steel ratio on the mechanisms of failure are discussed.