Recommendations for Concrete Members Prestressed With Unbonded Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommendations for Concrete Members Prestressed With Unbonded Tendons

Author(s): ACI-ASCE Committee 423

Publication: Structural Journal

Volume: 86

Issue: 3

Appears on pages(s): 301-318

Keywords: anchorage (structural); beams (supports); concrete construction; bond (concrete to reinforcement); concrete slabs; corrosion; cover; cracking (fracturing); earthquake-resistant structures; fire resistance; flat concrete plates; flat concrete slabs; joint

DOI: 10.14359/2918

Date: 5/1/1989

Abstract:
Report is presented as a guide for the design of flexural structural members in buildings with unbonded tendons. Suggestions are presented for needed revisions and additions to the ACI 318 Building Code regarding this subject. Consideration is given to determination of fire endurance, design for seismic forces, and catastrophic loadings, in addition to design for gravity and lateral loads. Recommendations are presented concerning details and properties of tendons, protection against corrosion, and construction procedures.