Title: Resolution of Field Problems With unbonded Single-Strand Tendons

Author(s): Gregory P. Chacos

Publication: Concrete International

Volume: 10

Issue: 2

Appears on pages(s): 40-44

Keywords: inspection; post-tensioning; prestressing steels; repairs; unbonded prestressing; Structural Research

DOI:

Date: 2/1/1988

Abstract:
Unbonded single-strand tendons and the most common field problems encountered with their use are described. Emphasis is placed on understanding the components of tendons and their abuse and malfunction. Repair methods are addressed briefly.