Design Related Distress in Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Related Distress in Concrete Pavements

Author(s): Jamshid M. Armaghani, Torbjorn J. Larsen and Lawrence L. Smith

Publication: Concrete International

Volume: 10

Issue: 8

Appears on pages(s): 43-49

Keywords: concrete pavements; cracking (fracturing); failure; inspection; structural design; subbases; Design

DOI:

Date: 8/1/1988

Abstract:
Discusses the cause of premature cracking in a concrete econocrete pavement system with unbonded interface, tiered and doweled joints, and variable length slabs with skewed joints. Results of tests, analyses, and field inspection of the pavement are presented.