Probabilistic Analysis of Cracking Moment of Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Probabilistic Analysis of Cracking Moment of Reinforced Concrete Beams

Author(s): Prakash Desayi and K. Balaji Rao

Publication: Structural Journal

Volume: 86

Issue: 3

Appears on pages(s): 235-241

Keywords: beams (supports); coefficient of variation; moments; cracking (fracturing); loads (forces); probability theory; reinforced concrete; structural analysis; Structural Research

DOI: 10.14359/2873

Date: 5/1/1989

Abstract:
Probabilistic analysis of cracking moment from 22 simply supported reinforced concrete beams is performed. When the basic variables follow the distribution considered in this study, the cracking moment of a beam is found to follow a normal distribution. An expression is derived, for characteristic cracking moment, which will be useful in examining reinforced concrete beams for a limit state of cracking.