Title: Deformation Properties and Ductility of High-Strength Concrete

Author(s): L. Bjerkeli, A. Tomaszewicz, and J. J. Jensen

Publication: Symposium Paper

Volume: 121

Issue:

Appears on pages(s): 215-238

Keywords: columns (supports); compressive strength; confined concrete; creep properties; deformation; ductility; high-strength concretes; lightweight concretes; reinforced concrete; reinforcing steels; stress-strain relationships; Structural Research

DOI: 10.14359/2844

Date: 11/1/1990

Abstract:
Paper summarizes results obtained as part of a recent research program on high-strength concrete (HSC). In this research, normal density concrete (mean cube strength of 65 to 115 MPa) and lightweight aggregate concrete (mean cube strength of 60 to 90 MPa)