Behavior of Exterior Reinforced Concrete Beam Column Joints Subjected to Bi-Directional Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Exterior Reinforced Concrete Beam Column Joints Subjected to Bi-Directional Cyclic Loading

Author(s): Zhu Bolong and Chen Yuzhou

Publication: Symposium Paper

Volume: 123

Issue:

Appears on pages(s): 69-96

Keywords: beams (supports), bending moments; joints (junctions); slabs; columns (supports), cyclic loads; ductility; reinforced concrete; shear properties; Structural Research

DOI: 10.14359/2815

Date: 1/1/1991

Abstract:
The results of three full-scale reinforced concrete beam-column joint specimens subjected to one- and two-directional reversed loading are presented in this paper. The influences on aseismic behavior of beam-column joints with different loading systems and monolithic slabs have been analyzed. Also, the relevant provisions for joints in the Chinese design code for reinforced concrete structures have been checked by test results, and some recommendations for beam-column joint design are given.