Size Effect in Punching Shear Failure of Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Size Effect in Punching Shear Failure of Slabs

Author(s): Zdenek P. Bazant and Zhiping Cao

Publication: Structural Journal

Volume: 84

Issue: 1

Appears on pages(s): 44-53

Keywords: concrete slabs; cracking (fracturing); ductility; failure; punching shear; reviews; strains; structural design; tests; Structural Research

DOI: 10.14359/2785

Date: 1/1/1987

Abstract:
Punching shear tests of geometrically similar reinforced concrete slabs of different sizes are carried out. The nominal shear stress at failure is not constant, as assumed in the current design formulas, but decreases as the slab size increases. The observed size effect in punching shear strength is approximately described by an improved design formula which uses the size-effect law for brittle failures due to distributed cracking. Applicability of this law is further supported by measurements of deflection diagrams, which reveal that the post-peak load decline becomes steeper as the slab size increases. Previous test data by various investigators are also analyzed collectively as one large set. Due to the enormity of scatter within this set, the absence of geometrical similarity and the lack of significantly different slab sizes within any single test series, these previous test data neither corroborate nor contradict the applicability of the size-effect law to punching shear.


ALSO AVAILABLE IN:

Electronic Structural Journal