Tower Structures Subjected to Temperature and Wind

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tower Structures Subjected to Temperature and Wind

Author(s): Piotr Noakowski and Kurt H. GerstleI

Publication: Structural Journal

Volume: 87

Issue: 4

Appears on pages(s): 479-487

Keywords: bending moments; chimneys; cooling towers; cracking (fracturing); crack width and spacing; deflection; moment-curvature relationships; reinforced concrete; stiffness; structural analysis; temperature; tension; thermal gradient; towers; wind pressure; Stru

DOI: 10.14359/2781

Date: 7/1/1990

Abstract:
A comparison study is presented of the analysis of ring sections of cylindrical tower structures subject to the effects of temperature gradient and wind loading. Five different assumptions were made regarding section stiffness, reflecting a number of approaches from U.S. and European practice, which lead to computations of a wide range of complexity. Results indicate that deflections and crack widths can only be predicted realistically if the sensitivity of temperature effects to stiffness is considered. The interaction between temperature effects and wind loading cannot be neglected. Regarding structure strength, redistribution of moments due to cracking increases the carrying capacity and should be considered. Suggestions are made regarding choice of assumptions for analysis, which strikes a reasonable compromise between reality and simplicity.