Site and Laboratory Evaluation of Repairs to Marine Concrete Structures and Maintenance Methodologies--Two Case Studies

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Site and Laboratory Evaluation of Repairs to Marine Concrete Structures and Maintenance Methodologies--Two Case Studies

Author(s): H. Roper, J. L. Heiman, and D. Baweja

Publication: Symposium Paper

Volume: 109

Issue:

Appears on pages(s): 563-586

Keywords: chlorides; concrete durability; corrosion; corrosion resistance; evaluation; maintenance; marine atmospheres; repairs; wharves; Structural Research

DOI: 10.14359/2755

Date: 8/1/1988

Abstract:
In Australia, the major population centers are located on the coast. A significant proportion of the nation's heavy industrial infrastructure and civil engineering work is also coastal. A wide variety of structures have been constructed in aggressive marine environments. Many of these structures have had long histories of durability problems and subsequent repair. Paper reports on field and laboratory studies that have been carried out to evaluate the performance of two wharf structures and their repair systems. It discusses the usefulness of various methods of detecting corrosion activity and considers the effects of chloride contamination and carbonation on damaged structures. Some aspects of repair materials for use in the marine environment are considered.