Effect of Curing Temperature and Humidity on Strength of Concrete Containing Blast-Furnace Slag Admixture

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Curing Temperature and Humidity on Strength of Concrete Containing Blast-Furnace Slag Admixture

Author(s): Taketo Uomoto and Kazusuke Kobayashi

Publication: Symposium Paper

Volume: 114

Issue:

Appears on pages(s): 1345-1360

Keywords: admixtures; age-strength relation; blast furnace slag; compressive strength; concretes; curing; humidity; slags; temperature; Materials Research

DOI: 10.14359/2605

Date: 5/1/1989

Abstract:
The compressive strength of blast furnace slag concrete containing slag/(cement + slag) ratios of 0, 0.3, 0.5, and 0.7 was followed by changing the curing conditions. The specimens were cured in air or water at 10, 20, or 40 C, and the strength development after 1, 4, 8, 13, and 26 weeks was determined. Equations were developed for strength based on maturity, curing, method, age of concrete, and amount of slag.