Development of Strength and Elastic Properties in Slag Cement Concretes Under Low Temperature Curing Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Strength and Elastic Properties in Slag Cement Concretes Under Low Temperature Curing Conditions

Author(s): D. E. Wimpenny, C. Ellis, C. M. Reeves, and D. D. Higgins

Publication: Symposium Paper

Volume: 114

Issue:

Appears on pages(s): 1283-1306

Keywords: age-strength relation; blast furnace slag; blended cements; compressive strength; concretes; curing; dynamic modulus of elasticity; flexural strength; low temperature; splitting tensile strength; slag cements; ultrasonic tests; Materials Research

DOI: 10.14359/2602

Date: 5/1/1989

Abstract:
Within-mixer blending of ground granulated blast furnace slag (GGBS) and ordinary portland cement (PC) to modify the hydration and durability characteristics of the cementitious binder is well established. Previous published work on the early strength development of concrete containing fly ash or slag has avoided combining low curing temperatures with low OPC content mixes, or has not applied the low temperatures continuously from casting. An investigation is in progress on the effects of low temperature (fixed and cycled) curing of concretes containing slags from two sources. The work examines the influence of a range of curing temperatures and mix proportions upon strength and elastic properties. This paper presents findings from the fixed temperature curing part of the research, in which specimens were manufactured from mixes with three cementitious contents and three OPC/GGBS blends at a constant water content.