Influence of Fiber Geometry in Steel Fiber Reinforced Dry-Mix Shotcrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Fiber Geometry in Steel Fiber Reinforced Dry-Mix Shotcrete

Author(s): Nemkumar Banthia, Jean-Francois Trottier, David Wood, and Denis Beaupre

Publication: Concrete International

Volume: 14

Issue: 5

Appears on pages(s): 24-28

Keywords: compressive strength; flexural strength; load-deflection curve; shotcrete; steel fibers; Materials Research

DOI:

Date: 5/1/1992

Abstract:
Discusses the influence of fiber geometry on the properties of steel fiber reinforced shotcrete. A laboratory investigation was carried out to understand the influence of fiber geometry on fiber rebound and hardened shotcrete properties. Five commercially available deformed fibers were selected. Fiber percent rebound was found to be closely related to a fiber geometrical parameter called the specific projected area.