Fire Resistance of High Strength/Dense Concrete With Particular Reference to the Use of Condensed Silica Fume--A Review

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fire Resistance of High Strength/Dense Concrete With Particular Reference to the Use of Condensed Silica Fume--A Review

Author(s): P. A. Jahren

Publication: Symposium Paper

Volume: 114

Issue:

Appears on pages(s): 1013-1050

Keywords: creep properties; fire resistance; high-strength concretes; lightweight concretes; moisture; porosity; prestressed concrete; reviews; silica fume; spalling; strains; stresses; temperature; Materials Research

DOI: 10.14359/2572

Date: 5/1/1989

Abstract:
Use of silica fume is an accepted technology in the Norwegian concrete environment and high-strength concrete incorporating silica fume is being used increasingly. However, in recent years, conflicting reports regarding the fire resistance of high-strength concrete have been published. This review indicates that eventual fire-safety problems seem to be linked less to the materials used than to physical properties of hardened concrete or conditions under which high strength concrete is used.