Title: Colored Concrete — Paving the Way for Beauty

Author(s): N. Paris and M. Chusid

Publication: Concrete International

Volume: 21

Issue: 7

Appears on pages(s): 22-25

Keywords: aesthetics; colors; durability; pavements; pigments; safety; solar radiation

DOI:

Date: 7/1/1999

Abstract:
Concrete is typically specified for pavements because of its strength, durability, and life-cycle value, Increasingly, it is also specified for another characteristic ! concrete’s good looks and aesthetic potential. No other paving material offers such a versatile design medium. Concrete pavement can be colored, textured and patterned to create almost any visual treatment a designer imagines. Patterned stamped colored concrete pavement can look like brick, stone work, boardwalk, and a wide variety of other finishes.