Rheological Analysis of the Behavior of Bleed Water from Freshly Cast Mortar and Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rheological Analysis of the Behavior of Bleed Water from Freshly Cast Mortar and Concrete

Author(s): M. Sawaide and J. Iketani

Publication: Materials Journal

Volume: 89

Issue: 4

Appears on pages(s): 323-327

Keywords: bleeding (concrete); capillarity; concretes; mortars (material); rheological properties; Materials Research

DOI: 10.14359/2549

Date: 7/1/1992

Abstract:
Analysis, based on Poiseville's law, of data on the changes in time seen in the depth of accumulation of the bleed water from freshly cast mortar and concrete indicated the existence of a relationship between this depth of bleed water accumulation and the time elapsed after addition of water to cement. Plots mutually relating these two variables proved to follow lines changing abruptly in character to mark three steps during the phase of bleed water exudation and two steps in the resorption phase.