Evaluation of the Use of Current Concrete Practice in the Production of High Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of the Use of Current Concrete Practice in the Production of High Strength Concrete

Author(s): P. M. Carrasquillo and R. L. Carrasquillo

Publication: Materials Journal

Volume: 85

Issue: 1

Appears on pages(s): 49-54

Keywords: capping; compressive strength; curing; evaluation; molds; flexural strength; high-strength concretes; plasticizers; quality control; specimens; Materials Research

DOI: 10.14359/2502

Date: 1/1/1988

Abstract:
A research program was conducted for the study of various quality-control procedures as applied to high-strength concrete. Over 1000 specimens for strength evaluation were cast from 29 high-strength concrete mixtures having compressive strengths ranging from 6000 to 14,500 psi at 28 days. Variables investigated included test specimen size, cylinder mold material, curing conditions, addition of superplasticizer, and cylinder capping method.