10,000 psi concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 10,000 psi concrete

Author(s): James E. Cook

Publication: Concrete International

Volume: 11

Issue: 10

Appears on pages(s): 67-75

Keywords: coarse aggregates; high-strength concretes; mix proportioning, modulus of electricity; quality control; skewness; tests; water-reducing agents; Materials Research

DOI:

Date: 10/1/1989

Abstract:
Approximately 85,000 yd3 of cast-in-place concrete, of which 21,000 yd3 were 10,000 psi concrete, were used to complete a 72-story building in Dallas, Tex. High-strength concrete was considered for this project because it met the architectural, engineering, and economic demands of the tall, slender structure. The data reported are results of extensive testing prior to the start of constrution. Evaluation of strength tests of field samples of concrete also are reported to show that quality-control techniques used for low to moderate strength concretes may not be appropriate for higher strength concretes.