Title: Getting What Was Asked for With High-Strength Concrete

Author(s): Bryce P. Simons

Publication: Concrete International

Volume: 11

Issue: 10

Appears on pages(s): 64-66

Keywords: concretes; field tests; high-strength concretes; laboratories; mix proportioning; performance; specifications; tests; Materials Research

DOI:

Date: 10/1/1989

Abstract:
Reading and understanding a set of project specifications dealing with high-strength concrete is fairly simple. Unfortunately, providing a material that successfully complies with all of the requirements throughout the course of a project is far more difficult. This article deals with the beginning aspects of developing a suitable high-strength concrete, including the initial work that must be done in the laboratory and subsequent field work.