Chemical Admixtures for Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Chemical Admixtures for Concrete

Author(s): ACI Committee 212

Publication: Materials Journal

Volume: 86

Issue: 3

Appears on pages(s): 297-327

Keywords: accelerating agents; adhesives; admixtures; bactericides; air-entraining agents; alkali-aggregate reactions; batching; concretes; calcium chlorides; colors (materials); corrosion inhibitors; expanding agents; flocculating; foaming agents; fungicides; pigm

DOI: 10.14359/2460

Date: 5/1/1989

Abstract:
This sixth report of ACI Committee 212, now named "Chemical Admixtures for Concrete," updates the previous reports of 1944, 1954, 1963, 1971, and 1981. Admixtures discussed herein are those known as chemical admixtures; finely divided mineral admixtures have been transferred to ACI Committee 226. Admixtures are classified into five groups: air-entraining, accelerating, water-reducing and set-controlling, admixtures for flowing concrete, and miscellaneous. "Preparation and batching," which had a separate chapter in the 1981 Report, is included in Chapter 1. Chapter 5, "Admixtures for flowing concrete," is new, representing technology that has matured since 1981. Those admixtures possessing properties identifiable with more than one group are discussed with the group that describes its most important effect on concrete.