Characterization of Radioactive Concrete by Petrographic and Physical Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Characterization of Radioactive Concrete by Petrographic and Physical Methods

Author(s): Alan D. Buck

Publication: Materials Journal

Volume: 85

Issue: 1

Appears on pages(s): 55-58

Keywords: concretes; cores; damage; nuclear reactors; petrography; physical tests; radioactivity; Materials Research

DOI: 10.14359/2442

Date: 1/1/1988

Abstract:
Portions of a core drilled from radioactive concrete in a dismantled German nuclear reactor were examined by petrographic methods and physical tests. While there was some indication of radiation damage by some of the physical testing, it was concluded from results of the petrographic examination that this was a specimen effect and that there was no radiation damage to the concrete.