Polymer Concrete Overlay

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Polymer Concrete Overlay

Author(s): Peter Mendis

Publication: Concrete International

Volume: 9

Issue: 12

Appears on pages(s): 54-56

Keywords: bonding; bridge decks; compressive strength; epoxy resins; electrical resistance; mixers; permeability; polymer concrete; screeds; resurfacing; skid resistance; tensile strength; Materials Research

DOI:

Date: 12/1/1987

Abstract:
The deck of New York City's historic Brooklyn Bridge was resurfaced with epoxy polymer concrete to protect the deck from further deterioration, to provide skid resistance, and to lower the noise level.