Title: Application of styrene-butadiene latex modified concrete

Author(s): Lou A. Kuhlmann

Publication: Concrete International

Volume: 9

Issue: 12

Appears on pages(s): 48-53

Keywords: bridges (structures); concretes; latex; mix proportioning; parking facilities; resurfacing; styrene-butadiene resins; Materials Research

DOI:

Date: 12/1/1987

Abstract:
Characteristics of concrete modified with styrene-butadiene latex are discussed, and application techniques are described. Several case histories are presented.